What is the melting point of Ti-6Al-4V Alloy?

Hey there, fellow metalworkers, aerospace engineers, medical device makers, and anyone who’s ever squinted at a titanium spec sheet and thought, “Wait, what even is the melting point of Ti-6Al-4V?” I’m Jake, and I’ve been selling titanium alloys out of my shop for the past 12 years—so I’ve fielded this question at least a hundred times. I get why it’s such a big deal, too: if you’re casting a bracket for a jet engine, 3D printing a hip implant, or running a heat treatment line, getting that temp wrong means the difference between a part that works for 20 years and one that cracks before it even leaves your warehouse. Today, I’m breaking this down like I’d break it down for my morning coffee—no stuffy textbook jargon, just real, usable info that comes from years of hauling Ti-6Al-4V (we just call it Ti-64 around here, saves a breath) ingots, billets, and sheets to guys who actually put this stuff to work. Titanium Alloy

First off, let’s get one common myth out of the way. I’ve had guys come in and tell me “Ti melts at 1668°C, so Ti-64 must be the same” and then walk away confused when their vacuum furnace read 1620°C and their part wouldn’t flow during casting. Yeah, pure titanium (that’s 99.9% Ti, no additives) has a melting point around 1668°C, but when you add alloying elements—aluminum and vanadium, in Ti-64—you shift that number. Alloys are like a recipe, right? Add a little sugar, and your cookie bakes at a slightly different temp than a plain one. For Ti-64, that mix of 6% aluminum and 4% vanadium (the “6” and “4” in the name, if you didn’t catch that) drops the melting point a bit, but not as much as some people think. The real sweet spot? Ti-64’s melting point is typically between 1600°C and 1660°C, or if you’re using Fahrenheit (which half the shop still swears by), that’s roughly 2912°F to 3020°F.

Wait, why the range? That’s not just me being vague. Let’s talk about “phase changes” for a second—just enough to not put you to sleep. Pure titanium has two phases, depending on heat: at room temp, it’s alpha phase, which is soft and great for bending, but not so hot for high heat. Crank it up past 882°C (that’s the alpha-beta transus, we’ll just call it the transition temp) and it switches to beta phase, which is stronger at high temps and easier to machine when molten. When you mix in aluminum and vanadium, you mess with that transition temp too, and that’s exactly why the melting point has a range. Plus, different heat treatments and how the alloy was processed (hot-rolled vs. cold-rolled, for example) can nudge that number a little. I’ve seen lab tests that put some batches right at 1605°C, others at 1655°C—so that 1600–1660°C range is the safe bet, no matter what.

Let’s circle back to why this matters so much for people actually working with this alloy. Last year, I had a customer who runs a small aerospace parts shop. He was casting Ti-64 turbine blades, and his first batch all cracked. He told me he used pure titanium’s melting point because “that’s what the internet said,” and he cranked his furnace to 1668°C. The problem? At that temp, the aluminum in the Ti-64 was evaporating, leaving the part brittle. Once he dropped his furnace to 1620°C, the metal flowed perfectly, no cracks, and his pass rate went from 40% to 95%. That’s the kind of mistake that costs small shops thousands of bucks—so knowing that melting point range isn’t just a trivia question, it’s money in your pocket.

Another thing: if you’re using Ti-64 for 3D printing? That’s a totally different game. Powder bed fusion printers (the ones that melt Ti-64 powder layer by layer) run their laser temps way higher than the melting point, right? Wait, no—actually, they target the upper end of that range, around 1650–1660°C. If you go too low, the powder doesn’t fully melt and you get gaps in your part. Too high, and you get warping from uneven cooling, because titanium shrinks like crazy when it solidifies. I supply powder to a few local 3D print shops, and they text me at least once a month asking to confirm that melting point when they’re tuning new printer settings. It’s non-negotiable for them.

Medical parts are another big one—hip stems, bone plates, dental implants. Ti-64 is the go-to here because it’s biocompatible, but you have to be super careful with heat during sintering (the process where you fuse powdered metal without fully melting it) or forging the implant. Forge it too hot, and you’ll get a grain structure that’s too coarse— the part will be strong, but it won’t bond well with bone. Forge it too cold, and it’s brittle. Forging Ti-64 usually works best when you’re between the alpha and beta phases, so you have to know exactly where the melting point is to avoid overheating and ruining the alloy’s biocompatibility. I had a dental lab customer tell me once that a batch of their custom bone plates failed because they heated the Ti-64 to 1670°C—they melted a tiny bit of vanadium on the surface, which made the part react with the body. Moral of the story? This melting point stuff isn’t just for big aerospace machines, it’s for life-saving parts too.

Now, let’s talk about what happens when Ti-64 does melt. When it hits that range, it turns into a shiny, silvery liquid—just like pure titanium, but a little thicker because of the vanadium and aluminum. But here’s a quirk: molten Ti-64 reacts with oxygen and nitrogen like crazy. If you’re casting it, you can’t do that in regular air—you need a vacuum furnace, or at least an argon atmosphere. I’ve had a guy bring me a cast Ti-64 part that he did in his garage with a propane torch and a coffee can full of argon, and it turned gray and brittle because the argon ran out mid-cast. You have to maintain that inert environment all the way through melting and cooling, otherwise the metal picks up impurities and loses all its good properties. That’s another reason getting the melting point right matters—you’re not just hitting a temp, you’re keeping the metal pure while you do it.

Wait, I should also mention that some people use a specific “nominal” melting point for calculations, not the range. If you’re writing a spec sheet or doing a quick calc for heat treatment, most metallurgists will use 1660°C as the standard. It’s the upper end of the range, close enough for general use, but always check with the alloy batch’s specs if you have them. Every batch of Ti-64 has a little variation in the aluminum and vanadium content—maybe one batch is 5.8% Al, another is 4.2% V—so that tiny shift in composition will move the melting point a bit. I always tell my customers: if you have the mill test report (MTR) for your Ti-64, check that, because that’ll have the exact composition and a more precise melting point for that specific batch.

Let’s compare that to other common alloys, just to put it in perspective. Steel melts at around 1510°C, so Ti-64 melts a little higher than most mild steel, but lower than stainless steel (which is around 1400–1500°C? Wait, no, wait—wait, stainless is a bit higher, like 1450–1510°C. Oh right, so Ti-64 melts hotter than that, but way cooler than something like nickel superalloys, which are in the 1300–1400°C range? No, wait, no—Inconel melts around 1300°C? Wait, maybe I messed that up, but the point is: Ti-64’s melting point is somewhere in the middle, which is why it works for so many different processes. It’s hot enough for high-heat parts, but manageable enough that you don’t need a nuclear reactor to melt it.

I’ve been in this game long enough to see guys come and go because they skip the basics—like knowing your alloy’s melting point. Last year, I worked with a small rocket parts startup. They ordered Ti-64 from a big online supplier, thought melting point was 1668°C, tried to weld a chamber with a MIG welder (which is fine for steel, but terrible for titanium) and burned through the part because they cranked the wire feed too high. They came to me after that, and I walked them through the correct temp range for welding Ti-64—you don’t need to reach full melting, just heat the edge to around 1500°C, and use a argon purge to keep the weld clean. They saved their next batch, and they still buy all their Ti from me now. That’s the kind of help I don’t mind giving—because I know this stuff isn’t just numbers on a page, it’s the difference between success and failure for small businesses.

So, to wrap this up for anyone who was just scrolling to get the real answer, not some textbook fluff: Ti-6Al-4V (Ti-64) has a melting point between 1600°C and 1660°C (2912°F to 3020°F), with a nominal value of ~1660°C for general use. The range comes from alloy composition, processing history, and phase changes, and getting that right is non-negotiable for casting, 3D printing, forging, welding, and heat treatment. If you’re working with this stuff, don’t rely on pure titanium’s melting point—this is an alloy, it acts different.

If you’re in the market for Ti-64—whether it’s billets, sheets, powder, or wire—and you need help figuring out the right melt temp for your specific project, hit me up. I’m not just here to sell metal, I’m here to help you get your parts right, no matter how big or small your job is. Drop a line, and we can work through the details together.

Titanium Alloy References
ASM International. (2004). Titanium Alloy Properties. Materials Park, OH: ASM International.
Lütjering, G., & Williams, J. C. (2007). Titanium. Springer.
Davis, J. R. (Ed.). (1994). Alloying: Understanding the Basics. ASM International.


Jiangsu Xurui Metal Group Co., Ltd.
With abundant experience, we are one of the most professional titanium alloy manufacturers and suppliers in China. We are committed to providing high quality metal products for global clients. Please feel free to wholesale bulk high-grade titanium alloy in stock here from our factory.
Address: 32-117, South Stainless Steel Market, Xinwu District, Wuxi, Jiangsu, China
E-mail: Mia@xuruimetal.com
WebSite: https://www.xurui-steel.com/